19X20H4AM3Д2C Stainless Steels

19X20H4AM3Д2C - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 19X20H4AM3Д2C grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.17 0.22
Si 1.10 1.50
Mn 0.30 0.80
P - 0.035
S - 0.020
Cr 18.50 20.00
Ni 4.30 4.90
Mo - -

19X20H4AM3Д2C - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 19X20H4AM3Д2C

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
693 (≥) 147 (≥) 11 24 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade 19X20H4AM3Д2C

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
714 (≥) 384 (≥) 11 21 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 221
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
151 921 811

Equivalent Grade

Equivalent Products

We can customize the production of 19X20H4AM3Д2C grade, contact us for the best solution.