1OX25H6ATMΦ Stainless Steels

1OX25H6ATMΦ - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 1OX25H6ATMΦ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 1.00
Mn - 0.80
P - 0.035
S - 0.020
Cr 23.50 26.00
Ni 5.00 6.50
Mo 1.30 1.80
Al - 0.18
Mg - 0.02

1OX25H6ATMΦ - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 1OX25H6ATMΦ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
471 (≥) 278 (≥) 12 12 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 133

Physical properties of grade 1OX25H6ATMΦ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
538 (≥) 472 (≥) 42 12 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 141
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
627 446 952

Equivalent Grade

Equivalent Products

We can customize the production of 1OX25H6ATMΦ grade, contact us for the best solution.
sales@specificsteel.com