316L Stainless Steels to G3067

316L - Specification & Application

  • G3067 - Stainless steel bars
  • G3077 - Stainless steel wire rods
  • G3076 - Stainless steel wires

Stainless steel wire rods

Chemical composition(wt.%) of 316L grade: to G3067

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.030
Ni 12.00 15.00
Cr 16.00 18.00
Mo 2.00 3.00

316L - Detail

Stainless steel wire rods

Mechanical properties of grade 316L G3067

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
666 (≥) 537 (≥) 34 31 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 331

Physical properties of grade 316L G3067

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
444 (≥) 688 (≥) 13 22 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 233
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
339 132 887

Equivalent Products

We can customize the production of 316L grade, contact us for the best solution.