AISI440A Stainless Steels

AISI440A - Specification & Application

AISI440A

Chemical composition(wt.%) of AISI440A grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.60 0.75
Si - 1.00
Mn - 1.00
P - 0.04
S - 0.03
Cr 16.0 18.0
Mo - 0.75

AISI440A - Detail

AISI440A

Mechanical properties of grade AISI440A

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
778 (≥) 187 (≥) 21 12 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade AISI440A

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
612 (≥) 693 (≥) 11 43 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 233
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
116 157 592