CNS 405 Stainless Steels to G3067

CNS 405 - Specification & Application

  • G3067 - Stainless steel bars
  • G3076 - Stainless steel wires

Stainless steel wires

Chemical composition(wt.%) of CNS 405 grade: to G3067

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.030
Ni - -
Cr 11.50 14.50
Mo - -
Al 0.10 0.30

CNS 405 - Detail

Stainless steel wires

Mechanical properties of grade CNS 405 G3067

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
618 (≥) 143 (≥) 11 14 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical properties of grade CNS 405 G3067

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
767 (≥) 387 (≥) 13 31 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 314
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
178 585 747