CNS 431 Stainless Steels to G3067

CNS 431 - Specification & Application

  • G3067 - Stainless steel bars

Stainless steel bars

Chemical composition(wt.%) of CNS 431 grade: to G3067

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.20
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.030
Ni 1.25 2.50
Cr 15.00 17.00
Mo - -

CNS 431 - Detail

Stainless steel bars

Mechanical properties of grade CNS 431 G3067

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
347 (≥) 357 (≥) 42 41 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 113

Physical properties of grade CNS 431 G3067

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
724 (≥) 395 (≥) 31 22 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 112
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
653 848 667

Equivalent Products

We can customize the production of CNS 431 grade, contact us for the best solution.