S31260 Stainless Steels

S31260 - Specification & Application

S31260

Chemical composition(wt.%) of S31260 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.75
Mn - 1
P 0.03 -
S 0.03 -
Cr 24.0 26.0
Ni 5.50 7.50
Mo 2.50 3.50
Cu 0.20 0.80
W 0.10 0.50
N 0.10 0.30

S31260 - Detail

S31260

Mechanical properties of grade S31260

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
346 (≥) 186 (≥) 11 12 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade S31260

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
837 (≥) 966 (≥) 44 13 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 122
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
747 882 546

Equivalent Products

We can customize the production of S31260 grade, contact us for the best solution.
sales@specificsteel.com