2367 Stainless Steels to SS 142367

2367 - Specification & Application

  • SS 142367 - Stainless steel - SS steel 2367

Stainless steel - SS steel 2367

Chemical composition(wt.%) of 2367 grade: to SS 142367

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.030
Cr 17.50 19.50
Ni 13.00 17.00
Mo 3.00 4.00

2367 - Detail

Stainless steel - SS steel 2367

Mechanical properties of grade 2367 SS 142367

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
519 (≥) 914 (≥) 11 23 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 234

Physical properties of grade 2367 SS 142367

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
789 (≥) 493 (≥) 41 13 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 443
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
644 873 128

Equivalent Products

We can customize the production of 2367 grade, contact us for the best solution.