2382 Stainless Steels to SS 142382

2382 - Specification & Application

  • SS 142382 - Ferritic stainless free-cutting steel

Ferritic stainless free-cutting steel

Chemical composition(wt.%) of 2382 grade: to SS 142382

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 0.50
P - 0.030
S 0.15 0.35
Cr 17.50 18.50
Ni - 1.00
Mo 2.00 2.50
Ti 0.30 1.00

2382 - Detail

Ferritic stainless free-cutting steel

Mechanical properties of grade 2382 SS 142382

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
657 (≥) 632 (≥) 34 13 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 422

Physical properties of grade 2382 SS 142382

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
925 (≥) 379 (≥) 23 34 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
635 723 443

Equivalent Products

We can customize the production of 2382 grade, contact us for the best solution.