2383 Stainless Steels to SS 142383

2383 - Specification & Application

  • SS 142383 - Ferritic-martensitic stainless free-cutting steel

Ferritic-martensitic stainless free-cutting steel

Chemical composition(wt.%) of 2383 grade: to SS 142383

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.10 0.17
Si - 1.00
Mn - 1.50
P - 0.06
S 0.15 0.35
Cr 16.00 18.00
Ni - 0.50
Mo - 0.60

2383 - Detail

Ferritic-martensitic stainless free-cutting steel

Mechanical properties of grade 2383 SS 142383

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
123 (≥) 341 (≥) 24 23 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade 2383 SS 142383

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
854 (≥) 229 (≥) 24 34 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 312
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
471 313 767

Equivalent Products

We can customize the production of 2383 grade, contact us for the best solution.