2388 Stainless Steels to SS 142388

2388 - Specification & Application

  • SS 142388 - Stainless steel - SS steel 2388

Stainless steel - SS steel 2388

Chemical composition(wt.%) of 2388 grade: to SS 142388

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.09
Si - 1.00
Mn - 1.00
P - 0.04
S - 0.03
Cr 16.00 18.00
Ni 6.70 7.75
Mo - -
Al 0.75 1.50

2388 - Detail

Stainless steel - SS steel 2388

Mechanical properties of grade 2388 SS 142388

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
356 (≥) 863 (≥) 42 33 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 421

Physical properties of grade 2388 SS 142388

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
468 (≥) 324 (≥) 41 33 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
313 813 698

Equivalent Products

We can customize the production of 2388 grade, contact us for the best solution.
sales@specificsteel.com