2584 Stainless Steels to SS 142584

2584 - Specification & Application

  • SS 142584 - Stainless steel - SS steel 2584

Stainless steel - SS steel 2584

Chemical composition(wt.%) of 2584 grade: to SS 142584

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.025
Si - 1.00
Mn - 2.00
P - 0.030
S - 0.025
Cr 26.00 28.00
Ni 30.00 34.00
Mo 3.00 4.00
Cu 0.60 1.40

2584 - Detail

Stainless steel - SS steel 2584

Mechanical properties of grade 2584 SS 142584

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
241 (≥) 459 (≥) 44 21 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 311

Physical properties of grade 2584 SS 142584

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
918 (≥) 736 (≥) 32 12 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 311
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
477 475 623

Equivalent Products

We can customize the production of 2584 grade, contact us for the best solution.