X2CrNiMoN17-13 Stainless Steels to ISO 9327-5 (1999)

X2CrNiMoN17-13 - Specification & Application

  • ISO 9327-5 (1999) - Steel forgings and rolled or forged bars for pressure purposes - Technical delivery conditions - Part 5: Stainless steels
  • ISO 9329-4 (1997) - Seamless steel tubes for pressure purposes - Technical delivery conditions - Part 4: Austenitic stainless steels
  • ISO 9330-6 (1997) - Welded steel tubes for pressure purposes - Technical delivery conditions - Part 6: Longitudinally welded austenitic stainless steel tubes
  • ISO 9328-5 - Steel plates and strips for pressure purposes - Technical delivery conditions - Part 5: Weldable fine grain steels, thermomechanically rolled

Welded steel tubes for pressure purposes - Technical delivery conditions - Part 6: Longitudinally welded austenitic stainless steel tubes

Chemical composition(wt.%) of X2CrNiMoN17-13 grade: to ISO 9327-5 (1999)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.030
Cr 16.50 18.50
Mo 11.50 14.50
Ni 2.50 3.00
N 0.12 0.22

X2CrNiMoN17-13 - Detail

Welded steel tubes for pressure purposes - Technical delivery conditions - Part 6: Longitudinally welded austenitic stainless steel tubes

Mechanical properties of grade X2CrNiMoN17-13 ISO 9327-5 (1999)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
575 (≥) 853 (≥) 43 14 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade X2CrNiMoN17-13 ISO 9327-5 (1999)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
449 (≥) 765 (≥) 21 11 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 442
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
484 687 958

Equivalent Products