X6CrNiWNbN16-16, 1.4945 Stainless Steels to EN 10302: 2008

X6CrNiWNbN16-16, 1.4945 - Specification & Application

  • EN 10302: 2008 - Creep resisting steels, nickel and cobalt alloys
  • EN 10088-1: 2005 - Stainless steels. List of stainless steels

Creep resisting steels, nickel and cobalt alloys

Chemical composition(wt.%) of X6CrNiWNbN16-16, 1.4945 grade: to EN 10302: 2008

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Si 0.30 0.60
Mn - 1.50
Cr 15.50 17.50
Nii 15.50 17.50
P - 0.035
S - 0.015
W 2.50 3.50
N 0.06 0.14
Nb - 1.20

X6CrNiWNbN16-16, 1.4945 - Detail

X6CrNiWNbN16-16, 1.4945 Creep resisting steels, nickel and cobalt alloys

Mechanical properties of grade X6CrNiWNbN16-16, 1.4945 EN 10302: 2008

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
136 (≥) 957 (≥) 44 33 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 233

Physical properties of grade X6CrNiWNbN16-16, 1.4945 EN 10302: 2008

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
771 (≥) 995 (≥) 31 42 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 122
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
534 785 665

Equivalent Grade

Equivalent Products

We can customize the production of X6CrNiWNbN16-16, 1.4945 grade, contact us for the best solution.