1Cr17Mn6Ni5N Stainless Steels to GB/T 1220 (1992)

1Cr17Mn6Ni5N - Specification & Application

  • GB/T 1220 (1992) - Stainless steel bars
  • GB/T 3280 (1992) - Cold rolled stainless steel sheets and plates
  • GB/T 4237 (1992) - Hot rolled stainless steel sheets and plates
  • GB/T 4239 (1991) - Cold rolled stainless steel and heat resisting steel strips
  • GB/T 4356 (2002) - Stainless steel wire rods

Nickel steel grade, instead of number 1 cr17ni7 and magnetism after cold working, used in railway vehicle, etc

Chemical composition(wt.%) of 1Cr17Mn6Ni5N grade: to GB/T 1220 (1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn 5.50 7.50
P - 0.060
S - 0.030
Ni 3.50 5.50
Cr 16.00 18.00
N - 0.2500

1Cr17Mn6Ni5N - Detail

Stainless and heat resisting steels
Austenitic stainless steel. Grade 1Cr17Mn6Ni5N was replaced by new designation 12Cr17Mn6Ni5N according to GB/T 20878 (2007)

Mechanical properties of grade 1Cr17Mn6Ni5N GB/T 1220 (1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
675 (≥) 235 (≥) 44 44 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 142

Physical properties of grade 1Cr17Mn6Ni5N GB/T 1220 (1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
242 (≥) 288 (≥) 22 12 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 112
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
844 884 421

Equivalent Grade

Equivalent Products

We can customize the production of 1Cr17Mn6Ni5N grade, contact us for the best solution.