Heat-resisting steel bars
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.15 | 0.28 | ||
Si | 0.75 | 1.25 | ||
Mn | 1.00 | 1.60 | ||
P | - | 0.35 | ||
S | - | 0.03 | ||
Ni | 10.50 | 12.50 | ||
Cr | 20.00 | 22.00 | ||
N | 0.15 | 0.30 |
2Cr21Ni12N
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
771 (≥) | 589 (≥) | 22 | 22 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 144 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
415 (≥) | 864 (≥) | 22 | 11 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 422 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
968 | 465 | 825 |