403Cb(ESR)
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.13 | 0.18 | ||
Si | - | 0.50 | ||
Mn | 0.40 | 0.60 | ||
P | - | 0.025 | ||
S | - | 0.010 | ||
Cr | 11.00 | 13.00 | ||
Mo | - | 0.20 | ||
Ni | - | 0.60 | ||
Nb | 0.15 | 0.25 | ||
V | - | 0.10 | ||
Pb | - | 0.005 | ||
Sn | - | 0.05 | ||
Al | - | 0.05 |
403Cb
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
485 (≥) | 572 (≥) | 34 | 44 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 234 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
962 (≥) | 838 (≥) | 43 | 44 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 332 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
763 | 181 | 913 |
We can customize the production of 403Cb(ESR) grade, contact us for the best solution.
–sales@specificsteel.com