Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.06 | ||
Mn | 4.00 | 6.00 | ||
Si | - | 1.00 | ||
P | - | 0.04 | ||
S | - | 0.03 | ||
Cr | 20.50 | 23.50 | ||
Ni | 11.50 | 13.50 | ||
Mo | 1.50 | 3.00 | ||
N | 0.20 | 0.40 | ||
Nb | 0.10 | 0.30 | ||
V | 0.10 | 0.30 |
Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
284 (≥) | 129 (≥) | 14 | 12 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 333 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
562 (≥) | 692 (≥) | 44 | 32 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 134 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
212 | 281 | 239 |