Classification and designation for superalloys and high temperature intermetallic materials
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.06 | 0.12 | ||
Cr | 20.0 | 23.0 | ||
Ni | 35.0 | 40.0 | ||
W | 2.50 | 3.50 | ||
Al | - | 0.50 | ||
Nb | 1.20 | 1.70 | ||
Ti | 0.70 | 1.20 | ||
Si | - | 0.80 | ||
Mn | - | 0.70 | ||
P | - | 0.030 | ||
S | - | 0.020 | ||
Ce | - | 0.05 |
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
128 (≥) | 521 (≥) | 12 | 14 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 133 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
633 (≥) | 321 (≥) | 44 | 43 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 331 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
146 | 237 | 923 |