CNS Standard heat resistant alloy and corrosion resistant alloy bar and plate type and chemical composition
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.10 | ||
Si | - | 0.50 | ||
Mn | - | 1.00 | ||
P | - | 0.030 | ||
S | - | 0.015 | ||
Cr | 14.00 | 17.00 | ||
Ni | 70.00 | - | ||
Cu | - | 0.50 | ||
Al | 0.90 | 1.50 | ||
Ti | 2.00 | 2.60 | ||
Fe | 5.00 | 9.00 |
CNS Standard heat resistant alloy and corrosion resistant alloy bar and plate type and chemical composition
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
478 (≥) | 278 (≥) | 13 | 23 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 131 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
549 (≥) | 525 (≥) | 41 | 14 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 311 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
613 | 491 | 512 |
We can customize the production of NCF751 grade, contact us for the best solution.
–sales@specificsteel.com