Nicrofer 3718 So* - Alloy DS* Stainless Steels

Nicrofer 3718 So* - Alloy DS* - Specification & Application

Nicrofer 3718 So* - Alloy DS*

Chemical composition(wt.%) of Nicrofer 3718 So* - Alloy DS* grade:

Elements Min.(≥) Max.(≤) Similar Remarks
Ni 35.0000 39.0000
Cr 17.0000 19.0000
C 1.9000 2.5000
Mn 0.8000 1.5000
Si 1.9000 2.5000
Cu - 0.5000
Ti - 0.2000
P - 0.0300
S - 0.0300

Nicrofer 3718 So* - Alloy DS* - Detail

Nicrofer 3718 So* - Alloy DS*

Mechanical properties of grade Nicrofer 3718 So* - Alloy DS*

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
933 (≥) 391 (≥) 34 43 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 242

Physical properties of grade Nicrofer 3718 So* - Alloy DS*

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
344 (≥) 946 (≥) 34 14 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 341
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
458 394 983
We can customize the production of Nicrofer 3718 So* - Alloy DS* grade, contact us for the best solution.