Heat resisting steels and nickel alloys
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.12 | ||
Si | 0.70 | 1.40 | ||
Mn | - | 1.00 | ||
P | - | 0.040 | ||
S | - | 0.015 | ||
Cr | 12.00 | 14.00 | ||
Ni | - | - | ||
Al | 0.70 | 1.20 |
Heat resisting steels and nickel alloys
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
743 (≥) | 372 (≥) | 31 | 23 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 133 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
546 (≥) | 979 (≥) | 21 | 31 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 412 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
831 | 826 | 589 |