Specification for nickel and nickel alloys: bar
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.10 | ||
Si | - | 0.50 | ||
Mn | - | 0.50 | ||
P | - | 0.015 | ||
S | - | 0.015 | ||
Cr | 20.00 | 23.00 | ||
Ni | 58.00 | - | ||
Mo | 8.00 | 10.00 | ||
Al | - | 0.40 | ||
Cu | - | - | ||
Ti | - | 0.40 | ||
Fe | - | 5.00 | ||
Co | - | 1.00 | ||
Nb+Ta | 3.15 | 4.15 |
Specification for nickel and nickel alloys: bar
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
286 (≥) | 216 (≥) | 42 | 23 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 422 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
335 (≥) | 819 (≥) | 44 | 34 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 422 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
182 | 713 | 527 |
We can customize the production of NA21 grade, contact us for the best solution.