Heat-resisting steel bars
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.22 | 0.30 | ||
Si | 1.40 | 2.20 | ||
Mn | 10.50 | 12.50 | ||
P | - | 0.35 | ||
S | - | 0.03 | ||
Cr | 17.00 | 19.00 | ||
N | 0.22 | 0.33 |
3Cr18Mn12Si2N
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
763 (≥) | 131 (≥) | 32 | 41 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 323 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
274 (≥) | 214 (≥) | 23 | 32 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 442 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
456 | 357 | 922 |