DIN 17240 (1976) Heat Resisting and Highly Heat Resisting Materials for Bolts and Nuts; Quality Specifications; Replaced by: DIN EN 10269:1999
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.18 | 0.24 | ||
Si | 0.10 | 0.50 | ||
Mn | 0.30 | 0.80 | ||
P | - | 0.0350 | ||
S | - | 0.0350 | ||
Ni | 0.30 | 0.80 | ||
Cr | 11.0 | 12.50 | ||
Mo | 0.80 | 1.20 | ||
V | 0.25 | 0.35 |
DIN 17240 (1976) Heat Resisting and Highly Heat Resisting Materials for Bolts and Nuts; Quality Specifications; Replaced by: DIN EN 10269:1999
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
473 (≥) | 279 (≥) | 21 | 21 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 334 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
882 (≥) | 185 (≥) | 22 | 34 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 144 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
817 | 437 | 616 |
We can customize the production of X 22 CrMoV 12-1 grade, contact us for the best solution.
–sales@specificsteel.com