A 582 S18200 Stainless Steels to A 582/A 582M (2012)

A 582 S18200 - Specification & Application

  • A 582/A 582M (2012) - Standard Specification for Free-Machining Stainless Steel Bars

Standard Specification for Free-Machining Stainless Steel Bars

Chemical composition(wt.%) of A 582 S18200 grade: to A 582/A 582M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Mn - 2.50
Si - 1.00
P - 0.04
S 0.15 -
Cr 17.50 19.50
Ni - -
Mo 1.50 2.50

A 582 S18200 - Detail

Standard Specification for Free-Machining Stainless Steel Bars

Mechanical properties of grade A 582 S18200 A 582/A 582M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
249 (≥) 665 (≥) 11 23 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 431

Physical properties of grade A 582 S18200 A 582/A 582M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
596 (≥) 733 (≥) 31 14 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
514 257 186

Equivalent Products