Steel, Corrosion and Heat-Resistant, Welded Tubing 12Cr - 8.5Ni - 0.30Cb - 1.1Ti - 2.0Cu Vacuum Induction Plus Consumable Electrode Vacuum Melted Solution Heat Treated, Precipitation Hardenable
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.02 | ||
Si | - | - | ||
Mn | - | - | ||
P | - | - | ||
S | - | - | ||
Ni | - | 8.50 | ||
Cr | - | 12.00 | ||
Al | - | - | ||
Cu | - | 2.00 | ||
Ti | - | 1.15 | ||
Fe | - | remaining | ||
Mo | - | - | ||
Co | - | - | ||
Nb | - | 0.38 | ||
B | - | 0.003 |
Steel, Corrosion and Heat-Resistant, Welded Tubing 12Cr - 8.5Ni - 0.30Cb - 1.1Ti - 2.0Cu Vacuum Induction Plus Consumable Electrode Vacuum Melted Solution Heat Treated, Precipitation Hardenable
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
938 (≥) | 469 (≥) | 34 | 22 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 224 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
487 (≥) | 575 (≥) | 14 | 22 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 114 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
531 | 422 | 736 |
We can customize the production of Custom 455 grade, contact us for the best solution.