Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.050 | ||
Si | - | 0.75 | ||
Mn | - | 2.00 | ||
P | - | 0.035 | ||
S | - | 0.025 | ||
Cr | 26.00 | 27.00 | ||
Mo | 1.30 | 2.00 | ||
Ni | 4.50 | 5.00 | ||
N | 0.05 | 0.20 |
Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
115 (≥) | 245 (≥) | 31 | 32 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 344 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
386 (≥) | 676 (≥) | 14 | 12 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 423 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
427 | 794 | 746 |
We can customize the production of Z5CND27-05Az grade, contact us for the best solution.
–sales@specificsteel.com