Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.01 | ||
Mn | - | 0.30 | ||
Si | - | 0.20 | ||
P | - | 0.025 | ||
S | - | 0.02 | ||
Cr | 28.00 | 30.00 | ||
Ni | 2.00 | 2.50 | ||
Mo | 3.50 | 4.20 | ||
N | - | 0.02 | ||
Cu | - | 0.15 |
Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
587 (≥) | 674 (≥) | 22 | 12 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 422 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
581 (≥) | 823 (≥) | 14 | 31 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 323 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
653 | 367 | 967 |