Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.04 | ||
Si | - | 0.80 | ||
Mn | - | 2.00 | ||
P | - | 0.035 | ||
S | - | 0.020 | ||
Cr | 17.00 | 19.00 | ||
Ni | 9.00 | 11.00 | ||
Mo | - | 0.30 | ||
W | - | 0.20 | ||
Ti | - | 0.20 |
Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
188 (≥) | 397 (≥) | 42 | 12 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 123 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
519 (≥) | 789 (≥) | 11 | 44 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 324 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
749 | 745 | 834 |