High temperature alloys and other special alloys
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.20 | ||
Cr | 12.0 | 14.0 | ||
Ni | 1.75 | 2.25 | ||
P | - | 0.020 | ||
S | - | 0.010 |
High temperature alloys and other special alloys
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
698 (≥) | 832 (≥) | 42 | 11 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 341 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
361 (≥) | 969 (≥) | 43 | 12 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 123 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
861 | 663 | 433 |
We can customize the production of 12-2W grade, contact us for the best solution.
–sales@specificsteel.com