K273 Special Alloy

Chemical composition%of the ladle analysis of gradeK273

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)Mo(%)W(%)N(%)B(%)Nb(%)Al(%)
0.75-0.900.30-1.004.50-6.00Max 0.04Max 0.0218.0-21.04.50-5.500.80-1.200.80-1.200.10-0.20Max 0.0050.65-0.85Max 0.05
K273

Mechanical properties of gradeK273

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
318(≥) 268(≥) 11 34 21 Solution and Aging,Annealing,Ausaging,Q+T,etc 132

Physical properties of grade K273

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
639(≥) 157(≥) 43 22 22 Solution and Aging,Annealing,Ausaging,Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
948 928 822

K273 Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

Equivalent Grade