X2CrNn2 Stainless Steels to BS EN 10028-7

X2CrNn2 - Specification & Application

  • BS EN 10028-7 - Flat products made of steels for pressure purposes - Part 7: Stainless steels
  • BS EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • BS EN 10088-2 - Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes
  • BS EN 10088-3 - Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
  • BS EN 10088-4 - Stainless steels - Part 4: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for construction purposes
  • BS EN 10088-5 - Stainless steels - Part 5: Technical delivery conditions for bars, rods, wire, sections and bright products of corrosion resisting steels for construction purposes
  • BS EN 10272 - Stainless steel bars for pressure purposes
  • BS EN 10296-2 (2005) - Welded circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel

Welded circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel

Chemical composition(wt.%) of X2CrNn2 grade: to BS EN 10028-7

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 1.50
P - 0.04
S - 0.015
Cr 10.50 12.50
Ni 0.30 1.00
Mo - -
N - 0.03

X2CrNn2 - Detail

Welded circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel

Mechanical properties of grade X2CrNn2 BS EN 10028-7

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
552 (≥) 636 (≥) 12 33 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade X2CrNn2 BS EN 10028-7

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
954 (≥) 971 (≥) 21 31 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 322
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
316 398 536

Equivalent Products

We can customize the production of X2CrNn2 grade, contact us for the best solution.