Corrosion Resisting Alloy AFNOR Z10 CNW17
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.07 | 0.12 | ||
Si | - | 1.00 | ||
Mn | - | 1.00 | ||
P | - | 0.040 | ||
S | - | 0.030 | ||
Cr | - | 16.00 | ||
Ni | - | 12.00 | ||
W | - | 2.50 | ||
Ti | 4X C / 0.80 | - | ||
B | 0.001 | 0.006 |
Corrosion Resisting Alloy AFNOR Z10 CNW17
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
336 (≥) | 629 (≥) | 23 | 12 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 422 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
155 (≥) | 188 (≥) | 34 | 12 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 421 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
486 | 747 | 197 |
We can customize the production of Z10CNW17 grade, contact us for the best solution.
–sales@specificsteel.com