C-5A Special Alloy

Chemical composition%of the ladle analysis of gradeC-5A

W(%)Co(%)Ti(%)Ta(%)
72.4-84.08.0-10.03.8-12.23.0-11.5
C-5A
Density / (g/cm ^ 3) : 11.5 ~ 12.9
Hardness HRA: 90.7 ~ 91.5
Bending strength/MPa: 1585 ~ 1930
Use for example: used for steel rough machining

Mechanical properties of gradeC-5A

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
268(≥) 168(≥) 31 22 12 Solution and Aging,Annealing,Ausaging,Q+T,etc 413

Physical properties of grade C-5A

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
237(≥) 641(≥) 41 34 21 Solution and Aging,Annealing,Ausaging,Q+T,etc 313
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
825 927 662

C-5A Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

Equivalent Grade