W7 Tool Die Steels to SAE J 437 (1970)

W7 - Specification & Application

  • SAE J 437 (1970) - Selection and heat treatment of tool and die steels
  • SAE J 438 (1970) - Tool and die steels

Tool and die steels

Chemical composition(wt.%) of W7 grade: to SAE J 437 (1970)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.95 1.10
Si 0.10 0.40
Mn 0.10 0.40
Cr 0.35 0.50
V 0.15 0.25

W7 - Detail

Tool and die steels

Mechanical properties of grade W7 SAE J 437 (1970)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
529 (≥) 877 (≥) 42 41 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 234

Physical properties of grade W7 SAE J 437 (1970)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
259 (≥) 916 (≥) 21 24 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 312
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
439 788 957

Equivalent Grade

Equivalent Products

We can customize the production of W7 grade, contact us for the best solution.