A 473 S32100 Stainless Steels to A 473 (2009)

A 473 S32100 - Specification & Application

  • A 473 (2009) - Stainless Steel Forgings

Stainless Steel Forgings

Chemical composition(wt.%) of A 473 S32100 grade: to A 473 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Mn - 2.00
Si - 1.00
P - 0.045
S - 0.03
Cr 17.00 19.00
Ni 9.00 12.00
N - 0.10

A 473 S32100 - Detail

Stainless Steel Forgings

Mechanical properties of grade A 473 S32100 A 473 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
548 (≥) 564 (≥) 42 42 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 442

Physical properties of grade A 473 S32100 A 473 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
375 (≥) 221 (≥) 11 13 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
849 342 811