Stellite 23 Tool Die Steels

Stellite 23 - Specification & Application

Stellite alloy

Chemical composition(wt.%) of Stellite 23 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.40
Si - 0.60
Mn - 0.30
Cr - 24.00
Ni - 2.00
Mo - -
Co remaining -
W - 5.00
Fe - 1.00

Stellite 23 - Detail

Stellite alloy

Mechanical properties of grade Stellite 23

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
478 (≥) 425 (≥) 12 31 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 342

Physical properties of grade Stellite 23

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
743 (≥) 633 (≥) 24 31 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 211
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
187 182 926