Chemical composition(wt.%) of NCF600 grade: to D 3531 (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 0.50
Mn - 1.00
P - 0.030
S - 0.015
Cr 14.00 17.00
Ni 72.00 -
Cu - 0.50
Al - -
Ti - -
Fe 6.00 10.00

NCF600 - Detail

Special alloys steel for chemical plant

Mechanical properties of grade NCF600 D 3531 (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
729 (≥) 415 (≥) 34 42 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical properties of grade NCF600 D 3531 (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
235 (≥) 591 (≥) 12 44 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
245 378 558