STR11 Stainless Steels to D 3731 (2002)

STR11 - Specification & Application

  • D 3731 (2002) - Heat - resisting steel bars

Heat - resisting steel bars

Chemical composition(wt.%) of STR11 grade: to D 3731 (2002)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.45 0.55
Si - 1.00
Mn - 2.00
P - 0.03
S - 0.03
Cr 7.50 9.50
Ni - 0.60
Mo - -
N - -
Cu - 0.30

STR11 - Detail

Heat - resisting steel bars

Mechanical properties of grade STR11 D 3731 (2002)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
491 (≥) 639 (≥) 44 14 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade STR11 D 3731 (2002)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
674 (≥) 534 (≥) 44 43 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
388 792 348

Equivalent Grade

Equivalent Products

We can customize the production of STR11 grade, contact us for the best solution.
sales@specificsteel.com