Nickel-base superalloy
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.15 | ||
Cr | 13.0 | 20.0 | ||
Mo | 3.5 | 5.0 | ||
Ni | - | Remainder | ||
Co | 13.0 | 20.0 | ||
Al | 2.5 | 3.25 | ||
Ti | 2.5 | 3.25 | ||
B | - | 0.01 | ||
Fe | - | 4.0 |
GH4146
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
295 (≥) | 962 (≥) | 34 | 21 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 442 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
969 (≥) | 565 (≥) | 42 | 23 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 234 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
196 | 523 | 783 |
We can customize the production of GH4146 grade, contact us for the best solution.
–sales@specificsteel.com