Iron-based Superalloy
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.06 | ||
Cr | - | 20.0 | ||
Mo | - | 1.5 | ||
Ni | - | 25.0 | ||
Nb | - | 0.8 | ||
Ti | - | 0.8 | ||
B | - | 0.01 | ||
Fe | - | Remainder | ||
Mn | - | 1.9 | ||
Ce | - | 0.05 |
GH1013
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
225 (≥) | 766 (≥) | 34 | 32 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 332 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
916 (≥) | 351 (≥) | 11 | 14 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 342 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
889 | 277 | 228 |
We can customize the production of GH1013 grade, contact us for the best solution.