GH1013 Superalloys

GH1013 - Specification & Application

Iron-based Superalloy

Chemical composition(wt.%) of GH1013 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Cr - 20.0
Mo - 1.5
Ni - 25.0
Nb - 0.8
Ti - 0.8
B - 0.01
Fe - Remainder
Mn - 1.9
Ce - 0.05

GH1013 - Detail

GH1013

Mechanical properties of grade GH1013

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
682 (≥) 478 (≥) 42 13 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 421

Physical properties of grade GH1013

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
469 (≥) 645 (≥) 11 42 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 343
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
353 965 393

Equivalent Grade

Equivalent Products

We can customize the production of GH1013 grade, contact us for the best solution.