Nickel steel grade, instead of number 1 cr17ni7 and magnetism after cold working, used in railway vehicle, etc
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.15 | ||
Si | - | 1.00 | ||
Mn | 5.50 | 7.50 | ||
P | - | 0.060 | ||
S | - | 0.030 | ||
Ni | 3.50 | 5.50 | ||
Cr | 16.00 | 18.00 | ||
N | - | 0.2500 |
Stainless and heat resisting steels
Austenitic stainless steel. Grade 1Cr17Mn6Ni5N was replaced by new designation 12Cr17Mn6Ni5N according to GB/T 20878 (2007)
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
415 (≥) | 376 (≥) | 23 | 34 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 244 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
662 (≥) | 599 (≥) | 31 | 23 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 433 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
669 | 513 | 352 |
We can customize the production of 1Cr17Mn6Ni5N grade, contact us for the best solution.