Ni-Fe-Cr Alloy Solid Solution Strengthened
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.02 | ||
Mn | - | 2.00 | ||
Si | - | 1.00 | ||
P | - | 0.02 | ||
S | - | 0.015 | ||
Cr | 26.00 | 28.00 | ||
Ni | 29.50 | 32.50 | ||
Mo | 3.00 | 4.00 | ||
Cu | 0.60 | 1.40 |
Ni-Fe-Cr Alloy Solid Solution Strengthened
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
638 (≥) | 336 (≥) | 43 | 43 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 421 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
494 (≥) | 215 (≥) | 24 | 12 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 442 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
621 | 231 | 668 |
We can customize the production of N08028 grade, contact us for the best solution.