SUH330 Stainless Steels

SUH330 - Specification & Application

CNS standard heat resistant steel plate of the steel grade and chemical composition

Chemical composition(wt.%) of SUH330 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.50
Mn - 2.00
P - 0.040
S - 0.030
Cr 14.00 17.00
Ni 33.00 37.00
Mo - -

SUH330 - Detail

CNS standard heat resistant steel plate of the steel grade and chemical composition

Mechanical properties of grade SUH330

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
296 (≥) 481 (≥) 12 14 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 421

Physical properties of grade SUH330

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
237 (≥) 819 (≥) 14 14 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 113
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
993 312 855

Equivalent Grade

Equivalent Products