Stainless steels - Chemical composition
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.02 | ||
Si | - | 0.70 | ||
Mn | - | 1.00 | ||
P | - | 0.035 | ||
S | - | 0.015 | ||
Cr | 19.50 | 20.50 | ||
Ni | 17.50 | 18.50 | ||
Mo | 6.00 | 7.00 | ||
N | 0.18 | 0.25 | ||
Cu | 0.50 | 1.00 |
Stainless steels - Chemical composition
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
826 (≥) | 977 (≥) | 23 | 41 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 441 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
998 (≥) | 321 (≥) | 32 | 22 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 212 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
425 | 157 | 275 |