Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.09 | 0.14 | ||
Si | - | 0.50 | ||
Mn | 0.50 | 0.80 | ||
P | - | 0.025 | ||
S | - | 0.025 | ||
Cr | 10.00 | 12.00 | ||
Ni | - | 0.60 | ||
Mo | 5.50 | 7.00 | ||
N | 0.10 | 0.20 |
Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
829 (≥) | 891 (≥) | 23 | 33 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 122 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
489 (≥) | 193 (≥) | 12 | 44 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 231 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
387 | 871 | 768 |
We can customize the production of 12X1182MΦ grade, contact us for the best solution.
–sales@specificsteel.com