Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.12 | ||
Si | 2.20 | 3.00 | ||
Mn | - | 1.50 | ||
P | - | 0.035 | ||
S | - | 0.020 | ||
Cr | 18.00 | 20.00 | ||
Ni | 13.50 | 15.50 | ||
Mo | 0.35 | 0.50 | ||
W | 1.60 | 2.00 | ||
V | 0.18 | 0.30 |
Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
189 (≥) | 915 (≥) | 31 | 23 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 324 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
437 (≥) | 215 (≥) | 41 | 41 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 234 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
295 | 346 | 174 |
We can customize the production of 12X20H14C2 grade, contact us for the best solution.