Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.03 | ||
Si | - | 0.75 | ||
Mn | 5.05 | 7.50 | ||
P | - | 0.045 | ||
S | - | 0.03 | ||
Cr | 16.0 | 18.0 | ||
Ni | 3.50 | 5.50 | ||
N | - | 0.25 |
Stainless and heat resisting steels
A 213/A 213M (2011) Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
611 (≥) | 387 (≥) | 41 | 23 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 134 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
134 (≥) | 488 (≥) | 14 | 12 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 224 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
446 | 274 | 681 |
We can customize the production of 201L grade, contact us for the best solution.